Tension correction:The shape of the processed substrate is poor, such as in the middle of the wave edge
Function: To make the plate shape flat
Electrostatic oiling:
Apply electrostatic oil to the tinplate sheets after production to prevent rusting and transportation scratches
Pinhole detector:
Both the tin plating production line and the shearing production line are equipped with pinhole testers, which can detect pinhole problems on the tinplate surface during the production process and select problematic tinplate
![]() |
Standard:ISO9001 Number:02623Q30981R0M Issue Date:2023-06-16 Expiry Date:2026-06-16 Scope/Range:tinplate Issued By:BTCC |
![]() |
Standard:ISO14001 Number:02623E30184R0M Issue Date:2023-06-16 Expiry Date:2026-06-15 Scope/Range:mill Issued By:BTCC |
![]() |
Standard:GB/T19001-2016 Number:02623Q30981R0M Issue Date:2023-06-16 Expiry Date:2026-06-15 Scope/Range:tinplate Issued By:BTCC |
![]() |
Standard:GJB9001C-2017 Number:0623J31346R0M Issue Date:2023-06-16 Expiry Date:2026-06-15 Scope/Range:tinplate Issued By:BTCC |
![]() |
Standard:GB/T24001 Number:02623E30184R0M Issue Date:2023-06-16 Expiry Date:2026-06-15 Scope/Range:MILL Issued By:BTCC |
Contact Person: Mrs. Betty Liu
Tel: 0086-13771045196